1 7 mil digikote 40 x 500 2 1 4 inch core glossy finish free shipping on orders of 1 or more rolls.
Tempurature 1 7 mil laminate.
Roll film 27 in width or smaller must be purchased in multiples of two.
Its low melt adhesive activates at 230 250 degrees f resulting in a stronger bond without risk of heat degradation of your more delicate projects.
Since some laminators are made outside the u s.
This lamination material is perfect for porous semi gloss and gloss paper even card stock.
3 mil 75 mic 5 mil 125 mic 7 mil 175 mic 10 mil 250 mic without a carrier 230 f 110 c 248 f 120 c 257 f 125 c 284 f 140 c.
Order online or call 972 245 7883 to speak with a sales rep.
However the 1 5mil thickness is an economical choice when applying laminate to print materials that are constructed of heavy paper or cardstock such as business cards flash card sets presentation folders and book or manual covers.
Digikote laminating film 1 7 mil glossy finish.
5 mil runs at 240º 275º.
Usi opti clear gloss 1 7 mil roll laminating film.
I have just received and tested my trulam 12 pouch laminator tl 320b and trulam 7 mil laminating pouches 9 x 11 5 lp07ltr.
If the material shows bubbles in the adhesive or a wavy irregular surface the temperature is too high.
My test paper was simple 20lb.
I called lamination depot and talked to a customer support person about my application and she suggested 7 mil pouches.
1 5 mil runs at 290º 315º.
And have show measurements in microns mic and centigrade c we have included those below for your reference.
They are constructed of a silicone resin with fiberglass fabric reinforcement.
In general however these are the temperature settings you would use.
1 7 mil 43 2 microns usually offered in professional grade films this thickness is used on material that needs to remain highly flexible.
10 mil runs at 220º 260º.
While not as strong as garolite g 9 sheets these sheets offer better arc resistance in dry environments and a higher level of electrical insulation.
1 5 mil 38 1 microns this thickness is commonly used in schools because it provides the most economical laminating solution.
After laminating if the pouch adhesive is still cloudy the laminating temperature is too low.
3 mil runs at 275º 300º.
1 7 mil runs at 220º 270º.
Why use digikote.
For example map books are often laminated using 1 7 mil film.
Copy paper printed using a standard hp ink jet printer.
3 mil runs at 220º 270º.
A large amount of film at a low price point.
Garolite g 7 withstands temperatures up to 425 f higher than any other grade of garolite.
D k group high temp pet gloss thermal laminate 1 7 mil 38 inches x 500 feet.
Garolite g 7 is sometimes called silicone grade laminate phenolic and.
195f temperature range.
For general purpose film.